Lionfish666
New member
Well I finally finished building my tanks, stand and got all the plumbing together.
(front removed for photo)
Did the water test and it all works as planned, that is until the Krylon fusion started peeling off the back glass. I read it was ok underwater but either I didn't apply it correctly or the large amount of flow going has made it peel off the glass. I am quite upset.
Unfortunately I painted it before glueing so some of the paint is under the silicon, going to be impossible to remove it without teardown. I was thinking peel back as much as I can then silicon over what is left, then place a black acrylic piece in front of the glass? Or will the pressure on this crack the glass?
Any ideas how I can fix this? I just want a black backing so the pipes are hidden.
(front removed for photo)
Did the water test and it all works as planned, that is until the Krylon fusion started peeling off the back glass. I read it was ok underwater but either I didn't apply it correctly or the large amount of flow going has made it peel off the glass. I am quite upset.
Unfortunately I painted it before glueing so some of the paint is under the silicon, going to be impossible to remove it without teardown. I was thinking peel back as much as I can then silicon over what is left, then place a black acrylic piece in front of the glass? Or will the pressure on this crack the glass?
Any ideas how I can fix this? I just want a black backing so the pipes are hidden.