Floyd R Turbo
Either busy or sleeping
Hey James, for the Formica laminate top, you have stated to use polished Formica. Does this mean a Gloss finish, or can a Matte finish be used?
I'm gonna leave that one up to James. That's a pretty nasty looking chip. You're saying that happened before the tank was ever used, then someone used it for a few years?
I know that any repairs you do are going to stress the acrylic more than it already is and may actually cause failure, and WO #16 would probably not be the best choice.
I'm thinking something like WO #40 or #42 and a strip adehered over the damaged spot, or something like that. Again, this is all a James question.
w/r to the resurfacing, is it really that badly scratched up after only a few years that you have to start with 120? Start with the highest grit (smallest grain) that you need in order to remove the scratch, and work up in grit from there. The tank I resurfaced had gravel scratches from a magfloat up and down the entire front in a zig-zag pattern and I started with 400 after 800 wasn't making headway, and those were really deep scratches.